MELTING POINT OF METALS, ETC.
| Names. | °Fahr. |
|---|---|
| Platina | 4590 |
| Antimony | 842 |
| Bismuth | 487 |
| Tin | 475 |
| Lead | 620 |
| Zinc | 700 |
| Cast Iron | 2100 |
| Gold | 2192 |
| Wrought Iron | 2900 |
| Steel | 2500 |
| Copper | 2000 |
| Glass | 2377 |
| Beeswax | 151 |
| Sulphur | 239 |
| Tallow | 92 |
| Silver | 1832 |
WEIGHT OF METALS
PER CUBIC FOOT.
| Lbs. | |
|---|---|
| Brass | 525 |
| Copper | 550 |
| Gold | 1210 |
| Iron, Cast | 450 |
| Iron, Wrought | 485 |
| Lead, cast | 710 |
| Silver | 655 |
| Steel | 490 |
| Tin, cast | 456 |
| Zinc | 450 |