2 ounces of plaster to a pound of metal;— walnut, which makes it like the curve.

[Footnote: The second part of this is quite obscure.]

735.

[Dried earth 16 pounds, 100 pounds of metal wet clay 20,—of wet 100,-half,- which increases 4 Ibs. of water,—1 of wax, 1 Ib. of metal, a little less,-the scrapings of linen with earth, measure for measure.] [Footnote: The translation is given literally, but the meaning is quite obscure.]

736.

Such as the mould is, so will the cast be.

737.

HOW CASTS OUGHT TO BE POLISHED.

Make a bunch of iron wire as thick as thread, and scrub them with [this and] water; hold a bowl underneath that it may not make a mud below.

HOW TO REMOVE THE ROUGH EDGES FROM BRONZE.