Perry Film Testing Machine

A film of paint is tested in the following manner: A piece of film one inch square is cut out and placed between the two metallic plates which hold the film immediately under the pressure tube. Mercury is run in from a burette through the side-neck and applies pressure upon the film by gravity. As the mercury is run in it rises of course in the tubes until this pressure becomes so great as to finally break the film. At this point the mercury will run out, and, falling upon the two insulated iron plates immediately below, will cause contact and close the circuit which rings an electric bell, which is a signal for the operator to shut off the inflow of mercury through the side-neck from the burette.

The pressure tube is also supplied with a piston which is made of a piece of thin iron wire having a disc attached to its lower end. As the mercury rises in the pressure tube this iron wire is pushed up, being very delicately counterpoised over a wheel. Upon the breaking of the film the mercury runs out, but upon falling upon the two iron plates underneath causes contact to be made, which causes the current to run through the pair of magnets before mentioned, which, becoming electrified, attract the piston in the pressure tube, giving a reading for the maximum height of the column of mercury.

Diagram of Perry Filmometer

[Open large scale image (49 kB).]

The supply of mercury being shut off, the operator is now in a position to determine the total sum of both the elasticity and ductility of the paint film, and also the pressure at which the film broke. The breaking pressure of course is read directly upon the pressure column, which is divided into centimeters as has been described above, the piston indicating the maximum height of the mercury column. What may be termed the elasticity of the film can now be calculated. As is perfectly evident, the film in stretching does so by distending from a flat surface to a curved or cup-like surface. If the pressure tube is calibrated in cubic centimeters reckoned from a flat surface where the film was introduced, the stretch of the paint film in distending from a flat surface to a curved surface may be determined. The cubic contents of the pressure tube and side-arm become increased, owing to the cup-like shape the paint film takes on. By subtracting the amount of mercury indicated by the piston in the pressure tube from the amount of mercury delivered from the burette, the amount contained in the distended paint film is obtained, which serves as a measure of elasticity. The temperature is a most important point to consider in running daily tests upon the filmometer. The tests made by the writer were conducted at 70 degrees Fahrenheit throughout.