. It is made by mixing twenty parts of well-washed and sifted sharp sand with two parts of litharge and one of freshly burned and slaked quicklime, in fine _dry_ powder. This is made into a putty, by mixing with linseed oil. It sets in a few hours, having the appearance of light stone; and we mention it, as it may be frequently employed with advantage in repairing broken stone-work (as steps), by filling up the missing parts. The employment of Roman cement, plaster, &c., for masonry work, hardly comes within the limits of Domestic Manipulation.

2504. Cement for Leather and Cloth

An adhesive material for uniting the parts of boots and shoes, and for the seams of articles of clothing, may be made thus:—Take one pound of gutta-percha, four ounces of India rubber, two ounces of pitch, one ounce of shellac, two ounces of oil. The ingredients are to be melted together, and used hot.

Go to Bed with the Lamb and Rise with the Lark.

2505. Birdlime

Take any quantity of linseed oil, say half a pint; put it into an old pot, or any vessel that will stand the fire without breaking—the vessel must not be more than one-third full; put it on a slow fire, stir it occasionally until it thickens as much as required; this will be known by cooling the stick in water, and trying it with the fingers. It is best to make it rather harder than for use. Then pour it into cold water. It can be brought back to the consistency required with a little Archangel tar.

2506. Anglo-Japanese Work