IX.—Iron filings160 ounces
Lime 80 ounces
Red lead 16 ounces
Alum  8 ounces
Sal ammoniac  2 ounces
X.—Clay 10 ounces
Iron filings  4 ounces
Salt  1 ounce
Borax  1 ounce
Black oxide of manganese  2 ounces
XI.—Mix:
Iron filings180 ounces
Lime 45 ounces
Salt  8 ounces
XII.—Mix:
Iron filings140 ounces
Hydraulic lime 20 ounces
Sand 25 ounces
Sal ammoniac  3 ounces

Either of these last two mixtures is made into a paste with strong vinegar just before use.

XIII.—Mix equal weights of zinc oxide and black oxide of manganese into a paste with water glass.

XIV.—Copal varnish, 15 parts; hydrated lime, 10 parts; glue de nerfs (of sinews), 5 parts; fat drying oil, 5 parts; {25} powdered turpentine, 3 parts; essence of turpentine, 2 parts. Dissolve the glue de nerfs on the water bath, add all the other substances, and triturate intimately.

XV.—Copal varnish, 15 parts; powdered turpentine, 3 parts; essence of turpentine, 2 parts; powdered fish glue, 3 parts; iron filings, 3 parts; ocher, 10 parts.

XVI.—To make a cement for cast iron, take 16 ounces cast-iron borings; 2 ounces sal ammoniac, and 1 ounce sulphur. Mix well and keep dry. When ready to use take 1 part of this powder to 20 parts of cast-iron borings and mix thoroughly into a stiff paste, adding a little water.

XVII.—Litharge2 parts
Boiled linseed oil2 parts
White lead1 part
Copal1 part

Heat together until of a uniform consistence and apply warm.

XVIII.—A cement for iron which is said to be perfectly waterproof and fireproof is made by working up a mixture of equal weights of red lead and litharge with glycerine till the mass is perfectly homogeneous and has the consistency of a glazier’s putty. This cement is said to answer well, even for very large iron vessels, and to be unsurpassable for stopping up cracks in large iron pans of steam pipes.

Cement For Metal, Glass, And Porcelain.