February 11th.

none injured.

Fig. 6.

One tube Cornish, 9ft. 9in. long, 4ft. 6in. diameter. Tube 2ft. 3in. diameter, 5/16 inch plates, 30 lbs. pressure. The boiler rent open at the bottom, and was thrown a considerable distance by the reaction of the issuing contents. The plates along the bottom were reduced by corrosion to 1/16 inch where in contact with the brickwork, so that the boiler was unable to bear the usual working pressure.

No.8. Durham. ([Fig. 7.])

February 12th.

2 killed, 1 injured.